logo
좋은 가격  온라인으로

제품 세부 정보

> 상품 >
열 교환 튜브
>
ASME SA179 Carbon Steel Seamless Tube Low Carbon Steel U Bend Heat Exchanger Tube

ASME SA179 Carbon Steel Seamless Tube Low Carbon Steel U Bend Heat Exchanger Tube

브랜드 이름: YUHONG
모델 번호: ASME SA179 탄소강 U 벤드 열교환기 튜브
MOQ: 1000KGS
포장에 대한 세부 사항: 플라스틱 캡과 함께 나무로 되는 케이스 /Iron Case/ 뭉치
지불 조건: 신용장, 티/티
상세 정보
원래 장소:
중국
인증:
ABS, GL, DNV, NK, PED, AD2000, GOST9941-81, CCS, ISO 9001-2008
제품명:
U밴드 튜브
보통품:
ASTM A179, ASME SA179
OD:
1/4", 3/8", 1/2", 5/8", 3/4", 1", 1.1/4" 등
두께:
BWG10-25
반지름:
관습 할 수 있습니다
끝:
일반 끝, 경 사진 끝
표면 상태:
오일, 블랙 페인팅
강조하다:
ASME SA179 탄소강 이음매 없는 튜브, ASME SA179 U 벤드 열교환기 튜브
제품 설명

ASTM A179 / ASME SA179 Carbon Steel Heat Exchanger Tube Seamless Steel U Bend Tube

 

 

ASME SA179 carbon steel seamless U-bend tubes are used in roughly 60–70% of all carbon steel shell-and-tube heat exchangers globally.

In the petrochemical, refinery, and power generation sectors, if the operating environment is non-corrosive or mildly corrosive and temperatures are below 400°C, SA179 is the default "workhorse" choice. Its high ductility (minimum elongation of 35%) allows it to be cold-bent into a tight 1.5D radius without cracking—something higher-strength carbon steels struggle with. So, SA179 is used because it bends reliably, not because it is the strongest.

 

 

Chemical Composition % of ASME SA179 Carbon Steel Seamless Tube U Bend Heat Exchanger Tube 

Element % C Mn P S
0.06-0.18 0.27-0.63 0.035 0.04

 

 

Material Mechanical Properties of ASTM A179 / ASME SA 179 Carbon Steel Seamless Tube

Yield Strength(MPa) Tensil Strength(MPa) Elogation(%)
≥180 ≥325 ≥35

 

 

Comparison with Similar Grades

Grade Standard Key Difference
SA179 ASME Cold-drawn, mandatory heat treatment, fine grain, higher ductility.
SA192 ASME Higher carbon (0.06–0.18% C), higher tensile (≥55 ksi), for boilers.
SA210 A1 ASME Medium-carbon steel (C ≤0.27%), higher strength, for boiler tubes.
EN 10216-2 P195 EN Similar low-carbon seamless, slightly different mechanicals.
JIS G3461 STB340 JIS Japanese equivalent; comparable properties.

 

 

Some clients require SSC and HIC tests for SA179 carbon steel tubes. Core reasons:

  1. Work-hardening at the bend – Cold bending raises the outer radius hardness above sour-service limits (NACE MR0175). SSC testing forces the mill to prove their post-bend heat treatment actually softens the bend apex, not just the straight legs.

  2. Steel cleanliness – SA179 has no mandatory inclusion control. HIC testing forces the steelmaker to use ultra-low-sulfur, calcium-treated steel so elongated MnS inclusions don't open into hydrogen-trapping voids during bending.

  3. Surface damage – Scratches from worn bending mandrels create stress-raisers. Testing finished bent coupons catches these defects that straight-tube MTRs never reveal.

  4. Heat treatment verification – Passing SSC/HIC proves the mill performed a full normalizing after bending, not just a cheap local stress-relief that leaves a vulnerable microstructure.

 

 

Applications
  • Feedwater Heaters (Power Generation)

  • Heat Exchanger

  • HVAC Chillers and Condensers (Comfort & Process Cooling)

  • Industrial Intercoolers and Aftercoolers

  • Marine Engineering

 

 